Silicon carbide ceramic retroreflector optic scan mirror parts
- Description
- Inquiry
Silicon carbide ceramic retroreflector optic scan mirror parts
Silicon carbide (SiC) ceramics have excellent characteristics such as strong oxidation resistance, high hardness, high thermal stability, high temperature strength, small thermal expansion coefficient, high thermal conductivity, thermal shock resistance and chemical corrosion resistance. Therefore, it is widely used in petrochemical, metallurgical machinery, aerospace, microelectronics, automobiles, steel and other fields, and gradually shows advantages that other special ceramics cannot match.
Silicon carbide ceramic retroreflector optic scan mirror parts
Features
The technical properties of silicon carbide are remarkably similar to those of diamond. It is one of the lightest, hardest and
strongest technical ceramic materials and has exceptional thermal conductivity, chemical resistance and low thermal expansion.* Extremely high hardness
* Wear resistant
* Corrosion resistant
* Lightweight – Low Density
* High thermal conductivity
* High Young’s modulus
* Low thermal expansion coefficient
* Chemically and thermally resistant
* Outstanding thermal shock resistance
* Refractive index greater than a diamond
strongest technical ceramic materials and has exceptional thermal conductivity, chemical resistance and low thermal expansion.* Extremely high hardness
* Wear resistant
* Corrosion resistant
* Lightweight – Low Density
* High thermal conductivity
* High Young’s modulus
* Low thermal expansion coefficient
* Chemically and thermally resistant
* Outstanding thermal shock resistance
* Refractive index greater than a diamond
Property | Unit | Silicon Carbide Ceramic |
Color | Black | |
Silicon Carbide content | % | ≥99.2 |
Mechanical Properties | ||
Density | g/cm3 | 3.08-3.16 |
Compressive Strength | MPa | >2500 |
Bending Strength | MPa | 400-490 |
Hardness | Kg /m m3 | >2550 |
Elastic Modulus | Gpa | ≥410 |
Thermal Properties | ||
Operating Temperature Max | °C | 1900 |
Thermal Expansion Coefficient | i /°C | 4.0 |
Thermal Conductivity | W/mK | 100-120 |
Poisson’s ratio | 0.16 |